Elastocem
Highly Flexible Cementitious Waterproofing Membrane

- For waterproofing water tanks, bathrooms, balconies, swimming pools, and rooftops.
- High flexibility, accommodates structural movement, and covers cracks.
- Can be applied on damp surfaces with excellent adhesion and no peeling issues.
- Durable and tear-resistant surface, can be used without additional overlaying.
- Surface can be easily painted or overcoated with other waterproofing systems.
- Non-toxic, safe for use in drinking water tanks.
CHARACTERISTICS | RESULTS | TEST METHOD |
---|---|---|
Appearance | Part A: White liquid Part B: Grey powder |
– |
Mixing Ratio | 1:2.5 (A:B) by weight | – |
Mixed Density | 1.9 ± 0.1 | ASTM D1475 |
Elongation | 100% – 150% | ASTM D412 |
Tensile Strength | >2.0 MPa | ASTM D412 |
Adhesion | >1.0 MPa | ASTM D4541 |
Water Penetration | None | – |
Working Temperature | 5-40 °C | – |
Pot life at 30 °C | 30-40 mins | – |
Use with potable water | yes | – |
PACKING | 35 kg / set |
---|---|
CONSUMPTION | 1.0 – 1.5 kg/ m2 / coat |
COVERAGE | 14.0 m2 / set(2 coats) |
Surface Preparation
• The surface must be strong, clean, and dry, free from oil, dust, rust, curing agents, paint, or any contaminants. The surface must be firm and not peeling. Cracks should be repaired with suitable materials, and the surface should be leveled with no standing water.
• For repair works with existing waterproofing systems, remove the old waterproofing layer before application to ensure the best performance of the new system.
• If the substrate is too dry, dampen it with water to cure the concrete before application, but make sure there is no standing water during the work.
Mixing
• Mix ELASTOCEM according to the specified ratio for maximum performance. Pour the powder into the liquid and mix thoroughly using a low-speed mixer (not exceeding 400 rpm) for 3–4 minutes. Let it sit briefly to release air bubbles before application.
• Avoid adding extra water into the mixture. Once mixed, the material should be used within 30–40 minutes.
Application
• Apply the mixture with a stiff brush at a rate of 1.0–1.5 kg/m². Each coat should not exceed 1 mm in thickness. Allow 2–3 hours for drying.
• Apply the second coat in the same way but perpendicular to the first coat. A sponge can be used to smoothen the surface finish.
• For spray or trowel applications, adjust the mixing ratio as appropriate for the application method.
Curing
• Protect the waterproofing layer from rain until fully hardened. Cure with moisture for 3–4 days.
• For water tanks, apply on the inner surface. The tank can be filled with water after 5–7 days, but rinse thoroughly with clean water before use.
• In bathrooms or swimming pools, tiles can be laid 3–5 days after application.
For additional questions
02- 569-1540, 099-165-1155, 099-492-4224
Clevcon Thailand Co., Ltd.
Clevcon (Thailand) Co., Ltd.
is the expert of chemical products for construction industry. We both manufacture and distribute a complete range of goods under the well known brand “Clevcon”.